Anilox: critical factors

1 One of the critical factors concerning anilox life is wall thickness. In most cases, a wall width between 4 and 6 microns is ideal. The post-engraving process of diamond polishing ensures flat and smooth wall-tops. This gives the blade the necessary support, as long...

Q and A with Brett Forehand